Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 585 MPa @Temperature 600 °C, Time 360000 sec |
84800 psi @Temperature 1110 °F, Time 100 hour |
Initial Stress |
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Rupture Strength | 585 MPa @Temperature 649 °C, Time 3.60e+6 sec |
84800 psi @Temperature 1200 °F, Time 1000 hour |
|
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |