Polymer Property : Rupture Strength = 8.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 8.50 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
1230 psi

@Temperature 1650 °F,
Time 10000 hour
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Rupture Strength 8.50 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
1230 psi

@Temperature 1650 °F,
Time 10000 hour
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Rupture Strength 8.50 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
1230 psi

@Temperature 1650 °F,
Time 10000 hour
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Rupture Strength 8.50 MPa

@Temperature 1000 °C,
Time 3.60e+7 sec
1230 psi

@Temperature 1830 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 25Cr/12Ni No. HR7
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..