Rupture Strength 40.0 MPa

@Temperature 700 °C,
Time 3.60e+7 sec
5800 psi

@Temperature 1290 °F,
Time 10000 hour
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r..
Rupture Strength 40.0 MPa

@Temperature 700 °C,
Time 3.60e+7 sec
5800 psi

@Temperature 1290 °F,
Time 10000 hour
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Rupture Strength 40.0 MPa

@Temperature 815 °C,
Time 36000 sec
5800 psi

@Temperature 1500 °F,
Time 10.0 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Rupture Strength 40.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
5800 psi

@Temperature 1560 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 34Ni/25Cr/Nb No. HR 33 Nb
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..