Mechanical Properties Metric English Comments
Rupture Strength 28.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
4060 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..
Rupture Strength 28.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
4060 psi

@Temperature 1380 °F,
Time 10000 hour
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r..
Rupture Strength 28.0 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
4060 psi

@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Rupture Strength 28.0 MPa

@Temperature 1040 °C,
Time 360000 sec
4060 psi

@Temperature 1900 °F,
Time 100 hour
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..
Rupture Strength 28.0 MPa

@Temperature 980 °C,
Time 3.60e+6 sec
4060 psi

@Temperature 1800 °F,
Time 1000 hour
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..