Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 206.8 MPa @Temperature 482 °C, Time 3.60e+6 sec |
30000 psi @Temperature 900 °F, Time 1000 hour |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |