Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 14.5 MPa @Temperature 950 °C, Time 3.60e+7 sec |
2100 psi @Temperature 1740 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 25Cr/20Ni No. HR6 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |