Polymer Property : Hardness, H358/30 = 218 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 218 MPa
31600 psi
ISO 2039-1
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Hardness, H358/30 218 MPa
31600 psi
ISO 2039-1
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..