Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp.. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl.. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl.. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Hardness, H358/30 | 99.0 MPa | 14400 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl.. |