Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 80.0 - 98.0 MPa | 11600 - 14200 psi | Average value: 86.5 MPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Hardness, H358/30 | 63.0 - 98.0 MPa | 9140 - 14200 psi | Average value: 86.3 MPa Grade Count:3 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |