Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00490 GPa | 0.711 ksi | DIN 53504 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00490 GPa | 0.711 ksi | DIN 53504 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
50% Modulus | 0.00490 GPa | 0.711 ksi | DIN 53504 |
Lubrizol ESTANE® 58197 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00490 GPa | 0.711 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
50% Modulus | 0.00490 GPa | 0.711 ksi | DIN 53504 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |