Polymer Property : 50% Modulus = 0.00490 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.00490 GPa
0.711 ksi
DIN 53504
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00490 GPa
0.711 ksi
DIN 53504
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade)
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible..
50% Modulus 0.00490 GPa
0.711 ksi
DIN 53504
Lubrizol ESTANE® 58197 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00490 GPa
0.711 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
50% Modulus 0.00490 GPa
0.711 ksi
DIN 53504
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..