Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00350 GPa | 0.508 ksi | DIN 53504 |
Lubrizol ESTANE® T5275 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00350 GPa | 0.508 ksi | |
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middl.. |
|||
50% Modulus | 0.00350 GPa | 0.508 ksi | ISO 37 |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00350 GPa | 0.508 ksi | ISO 37 |
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00350 GPa | 0.508 ksi | DIN 53504 |
Lubrizol ESTANE® T5192 Ether-Type Dissipative Compound (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00350 GPa | 0.508 ksi | DIN 53504 |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |