Polymer Property : 50% Modulus = 0.0152 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Toyobo PELPRENE™ P90BD Polyester TPE, High Viscous, High Durability
Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo.
50% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
50% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR5760 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..