C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer , Polyurethane, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 20 Standard Adipate Ester: These products are based on saturated polyesters. They exhibit strength and durability with excellent tear and abrasion resistance; good hydrolytic stability resistance to solvents, oxidation and UV light degradation.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield 63.2 MPa
9170 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
50% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
100% Modulus 0.0175 GPa
2.54 ksi
ASTM D412
300% Modulus 0.0380 GPa
5.51 ksi
ASTM D412
Flexural Modulus 0.180 GPa
26.1 ksi
ASTM D790
Tear Strength 160 kN/m
913 pli
ASTM D624
Abrasion 40
40
mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 46.0 MPa
6670 psi
+20°C; ASTM D1043
354 MPa
51300 psi
-20°C; ASTM D1043
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525