Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0109 GPa | 1.58 ksi | ASTM D638 |
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |