50% Modulus 0.00570 GPa
0.827 ksi
DIN 53504
Lubrizol ESTANE® T5134 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00570 GPa
0.827 ksi
DIN 53504
Lubrizol ESTANE® 5712F30 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00570 GPa
0.827 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P High Hardness Extruded Profile
FormulationNordel® IP 4725P