Mechanical Properties Metric English Comments
50% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
Network Polymers Softflex® 7000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
50% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.