Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 60.0 - 800 MPa
8700 - 116000 psi
Average value: 388 MPa Grade Count:12
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Tensile Creep Modulus, 1000 hours 60.0 MPa
8700 psi
At 1% Deformation; DIN 53444
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Tensile Creep Modulus, 1000 hours 60.0 - 200 MPa
8700 - 29000 psi
Average value: 113 MPa Grade Count:4
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..