Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 500 - 850 MPa
72500 - 123000 psi
Average value: 570 MPa Grade Count:5
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Tensile Creep Modulus, 1000 hours <= 500 MPa
<= 72500 psi
DIN 53444
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..
Tensile Creep Modulus, 1000 hours <= 500 MPa
<= 72500 psi
DIN 53444
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
DSM Stanyl® TE341 Nylon 46 (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
BASF Ultraform® N2650 Z4 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Tensile Creep Modulus, 1000 hours 500 MPa

@Strain <=0.500 %
72500 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® N2650 Z6 POM + PUR