Polymer Property : Tensile Creep Modulus, 1000 hours = 4300 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4300 MPa
624000 psi
At 1% Deformation; DIN 53444
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
Tensile Creep Modulus, 1000 hours 4300 MPa

@Strain <=0.500 %
624000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Tensile Creep Modulus, 1000 hours 4300 MPa

@Strain <=0.500 %
624000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Tensile Creep Modulus, 1000 hours 4300 MPa

@Strain <=0.500 %
624000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry)
Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo..