Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 4300 MPa | 624000 psi | At 1% Deformation; DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |
|||
Tensile Creep Modulus, 1000 hours | 4300 MPa @Strain <=0.500 % |
624000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Tensile Creep Modulus, 1000 hours | 4300 MPa @Strain <=0.500 % |
624000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Tensile Creep Modulus, 1000 hours | 4300 MPa @Strain <=0.500 % |
624000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |