Polymer Property : Tensile Creep Modulus, 1000 hours = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 40.0 MPa

@Time 3.60e+6 sec
5800 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Creep Modulus, 1000 hours 40.0 MPa

@Time 3.60e+6 sec
5800 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers
Tensile Creep Modulus, 1000 hours 40.0 MPa

@Temperature 120 °C
5800 psi

@Temperature 248 °F
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide