Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 2100 - 5800 MPa | 305000 - 841000 psi | Average value: 3850 MPa Grade Count:4 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Tensile Creep Modulus, 1000 hours | 2100 MPa @Time 3.60e+6 sec |
305000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 2100 MPa @Strain <=0.500 % |
305000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Tensile Creep Modulus, 1000 hours | 2100 MPa @Strain <=0.500 % |
305000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Tensile Creep Modulus, 1000 hours | 2100 MPa @Strain <=0.500 % |
305000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Tensile Creep Modulus, 1000 hours | 2100 MPa @Strain <=0.500 % |
305000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |