Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 3.71 N/tex | 42.0 g/denier | |
Toyobo Zylon® AS Poly(p-phenylene-2,6-benzobisoxazole) Fiber Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using t.. |
|||
Tenacity | 3.71 N/tex | 42.0 g/denier | |
Toyobo Zylon® HM Poly(p-phenylene-2,6-benzobisoxazole) Fiber Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using t.. |