Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.300 - 0.335 N/tex | 3.40 - 3.80 g/denier | |
Intercontinental Polymers Deniers 15 Polyester Staple Fiber, Denier 15 Cut Lengths (Inches): 1, 1.25, 1.75, 2, 3 & 4. Lusters: Bright and Semi-Dull. Cross-Section: Round. Specialties: Optical Black, Spun-Dyed Black, Flame Retardant (US and European Standards), Cati.. |