Polymer Property : Tenacity = 0.300 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.300 - 0.335 N/tex
3.40 - 3.80 g/denier
Intercontinental Polymers Deniers 15 Polyester Staple Fiber, Denier 15
Cut Lengths (Inches): 1, 1.25, 1.75, 2, 3 & 4. Lusters: Bright and Semi-Dull. Cross-Section: Round. Specialties: Optical Black, Spun-Dyed Black, Flame Retardant (US and European Standards), Cati..
Tenacity 0.300 N/tex
3.40 g/denier
Knot Strength
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 2 mm)
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic..
Tenacity 0.300 - 0.500 N/tex
3.40 - 5.66 g/denier
Cathay Terryl® Renewable Engineering Polyamide
Terryl® provides significant advantages in spinnability, dyeability, water absorption and comfort.Information provided by Cathay