Mechanical Properties Metric English Comments
Tenacity 0.318 N/tex
3.60 g/denier
Knot Strength
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5.5)
Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE.
Tenacity 0.318 N/tex
3.60 g/denier
Knot Strength
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE.