Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.318 N/tex | 3.60 g/denier | Knot Strength |
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5.5) Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE. |
|||
Tenacity | 0.318 N/tex | 3.60 g/denier | Knot Strength |
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5) Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE. |