Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 2.12 N/tex | 24.0 g/denier | Tensile Modulus |
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.5) Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE. |
|||
Tenacity | 2.12 N/tex | 24.0 g/denier | Tensile Modulus |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.8) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |