Polymer Property : Tenacity = 2.12 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 2.12 N/tex
24.0 g/denier
Tensile Modulus
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.5)
Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE.
Tenacity 2.12 N/tex
24.0 g/denier
Tensile Modulus
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.8)
Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t..