Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.256 N/tex | 2.90 g/denier | Knot Strength |
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=4.5) Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | ASTM D3218 |
Total PPH M3865 Metallocene Isostatic Propylene Polymer, Fiber Grade M3865 is an isostatic form of polypropylene made via ATOFINA proprietary technology.Recommended Applications. M3865 is recommended for melt spun and spunbond fiber applications. However, due to it.. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | Straight test - filament yarn tested at 3 TPI, 10 inch gauge length and 60%/min extension rate. DuPont Test Method 12002 |
DuPont™ Nomex® 450 Aramid Staple Fiber A natural staple fiber. It has higher crystallinity and strength than Type 455 and 462 fibers, and is sold as a 100% meta-aramid staple in various cut lengths. It is used in applications requiring.. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | 3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256 |
Braskem D180M Homopolymer Polypropylene Description: Low Gas FadeApplications: Suggested Uses Include BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis resin meets the requirements for olefin polym.. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | 3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256 |
Braskem D180A2 Homopolymer Polypropylene Description: Excellent Melt StabilityApplications: Suggested Uses Include Caps and Closures, Housewares, BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis re.. |
|||
Tenacity | 0.256 N/tex | 2.90 g/denier | process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |