Material Notes:
DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50 mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ASTM D638
Tenacity 0.256 N/tex
2.90 g/denier
process conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 164 °C
327 °F
by DSC