Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.203 - 0.441 N/tex | 2.30 - 5.00 g/denier | Average value: 0.308 N/tex Grade Count:8 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tenacity | 0.203 N/tex | 2.30 g/denier | Dry |
Toho Tenax Pyromex® CPX 2d 312K Non-crimped Carbon Fiber Pyromex® is an oxidized organic polyacrylonitrile (PAN) fiber with excellent heat and flame resistance. It also features excellent resistance to chemicals and good electrical insulation properties.. |
|||
Tenacity | 0.203 N/tex | 2.30 g/denier | Dry |
Toho Tenax Pyromex® PX 2d Crimped Carbon Fiber Pyromex® is an oxidized organic polyacrylonitrile (PAN) fiber with excellent heat and flame resistance. It also features excellent resistance to chemicals and good electrical insulation properties.. |
|||
Tenacity | 0.203 N/tex | 2.30 g/denier | ASTM D3218 |
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns Process Stability TOTAL Petrochemicals Polypropylene 3764 features excellent processability and gas fade resistance.FDA. 3764 complies with all applicable FDA regulations for food contact applicat.. |
|||
Tenacity | 0.203 N/tex | 2.30 g/denier | 3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256 |
Braskem CP360H Homopolymer Polypropylene Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo.. |