Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.168 - 0.353 N/tex | 1.90 - 4.00 g/denier | Average value: 0.255 N/tex Grade Count:14 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |