Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 130 °C
266 °F
Hyosung Topilene C600M PP
C600M Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Low sealProcessabilityInformation provided by Hyosung Corporation
Heat Seal Strength Initiation Temperature 130 °C
266 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 130 °C
266 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th..
Heat Seal Strength Initiation Temperature 130 °C
266 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 130 - 180 °C
266 - 356 °F
BiologiQ ESR-PE EcoStarch mLLDPE Blend
Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ