Hyosung Topilene C600M PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene C600M PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C600M Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Low sealProcessabilityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.785 GPa
114 ksi
ASTM D790
Izod Impact, Unnotched 0.637 J/cm
1.19 ft-lb/in
ASTM D256
Heat Seal Strength Initiation Temperature 130 °C
266 °F
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
HS Method
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 120 °C
248 °F
ASTM D1525