Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 120 - 200 °C | 248 - 392 °F | |
DuPont Teijin Films Melinex® CORE 2 Polyester Film Melinex® CORE 2 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well.. |