Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.350 GPa | 50.8 ksi | 0.05-1.05%; ASTM D882-A |
Borealis Borstar® FB4230 LLDPE for Film Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar .. |