Secant Modulus, TD 0.350 GPa
50.8 ksi
0.05-1.05%; ASTM D882-A
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..