Mechanical Properties Metric English Comments
Secant Modulus, TD 0.221 - 0.238 GPa
32.0 - 34.5 ksi
Average value: 0.234 GPa Grade Count:5
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..