Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.415 GPa | 205.2 ksi | ASTM D882 |
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Secant Modulus, TD | 1.415 GPa | 205.2 ksi | ASTM D882 |
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness... |