Secant Modulus, TD 0.840 GPa
122 ksi
ASTM D882
Chevron Phillips HiD® 9605D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Secant Modulus, TD 0.840 GPa
122 ksi
ASTM D882
Chevron Phillips HiD® 9607D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Secant Modulus, TD 0.840 GPa
122 ksi
ASTM D882
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Secant Modulus, TD 0.840 GPa
122 ksi
ASTM D882
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..