Polymer Property : Secant Modulus, TD = 0.283 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.283 GPa
41.0 ksi
1% Strain; ASTM D882
M. Holland Company LL104 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..