Mechanical Properties Metric English Comments
Secant Modulus, TD 0.241 GPa
35.0 ksi
value @ 0.1 mm/mm-min Initial strain rate; ASTM D-882
Bapolene® 222F Polyethylene, Film Grade
Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a..