Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, TD = 0.240 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.240 GPa
34.8 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
Secant Modulus, TD 0.240 GPa
34.8 ksi
ASTM D882
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Secant Modulus, TD 0.240 GPa
34.8 ksi
ASTM D882
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b..
Secant Modulus, TD 0.240 GPa
34.8 ksi
ASTM D882
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer.
Secant Modulus, TD 0.240 GPa
34.8 ksi
ASTM D882
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic..
Secant Modulus, TD 0.240 GPa
34.8 ksi
ASTM D882
Chevron Phillips 5497 LDPE High Clarity, Bakery Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Openability, Suited for High Speed Converting, Good Clarity. Slip 1000 ppm. Antiblock 10000 ppm.Applications:Bakery Film, Bread BagsProcessing Con..
Secant Modulus, TD 0.240 GPa
34.8 ksi
0.01; ASTM D882
Eastman E6838-902F Polyethylene Film  (discontinued **)
Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business ..
Secant Modulus, TD 0.240 GPa
34.8 ksi
1% Secant; ASTM D882
Eastman 1830F Polyethylene  (discontinued **)
Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and..
Secant Modulus, TD 0.240 GPa
34.8 ksi
1% Secant; ASTM D882
Eastman E6838-922F Polyethylene  (discontinued **)
E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat..
Secant Modulus, TD 0.240 GPa
34.8 ksi
1% Secant; ASTM D882
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..