Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.200 - 0.230 GPa | 29.0 - 33.4 ksi | Average value: 0.208 GPa Grade Count:4 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |