Mechanical Properties Metric English Comments
Secant Modulus, TD 0.227 GPa
32.9 ksi
0.01; ASTM D882
Eastman 1550F Film Polyethylene  (discontinued **)
Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long..