Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, TD = 0.0970 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.0970 GPa
14.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring ..
Secant Modulus, TD 0.0970 GPa
14.1 ksi
2% Secant; ASTM D882
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..
Secant Modulus, TD 0.0970 GPa
14.1 ksi
ASTM D882
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell..