Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0960 GPa | 13.9 ksi | 2% Secant; ASTM D882 |
Dow INTEGRALâ„¢ 900 Deep Draw Multilayer Adhesive Film INTEGRAL 900 Adhesive Film is a heat-activated, moldable, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethan.. |