Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INTEGRAL™ 900 Deep Draw Multilayer Adhesive Film

Category Polymer , Film , Thermoset
Manufacturer Dow Chemical
Trade Name INTEGRAL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INTEGRAL™ 900 Deep Draw Multilayer Adhesive Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INTEGRAL 900 Adhesive Film is a heat-activated, moldable, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethanes.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 430 %
430 %
ASTM D882
Film Elongation at Break, TD 490 %
490 %
ASTM D882
Secant Modulus, MD 0.0900 GPa
13.1 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.0960 GPa
13.9 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 11.8 g/micron
300 g/mil
ASTM D882
Elmendorf Tear Strength, TD 16.1 g/micron
410 g/mil
ASTM D882
Film Tensile Strength at Break, MD 23.4 MPa
3400 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Users viewing this material also viewed the following: